SA-240 S44500 Stainless Steels to SA-240/SA-240M

SA-240 S44500 - Specification & Application

  • SA-240/SA-240M - Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of SA-240 S44500 grade: to SA-240/SA-240M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.012
Cr 19.00 21.00
Ni - 0.60
Mo - -
N - 0.03
Cu 0.30 0.60

SA-240 S44500 - Detail

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade SA-240 S44500 SA-240/SA-240M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
324 (≥) 961 (≥) 14 24 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade SA-240 S44500 SA-240/SA-240M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
896 (≥) 256 (≥) 13 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
893 152 784

Equivalent Products

We can customize the production of SA-240 S44500 grade, contact us for the best solution.