SA-693 S35000 Stainless Steels to SA-693

SA-693 S35000 - Specification & Application

  • SA-693 - Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of SA-693 S35000 grade: to SA-693

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.07 0.11
Mn 0.50 1.25
Si - 0.50
P - 0.04
S - 0.03
Cr 16.00 17.00
Ni 4.00 5.00
Mo 0.50 1.25
N 0.07 0.13

SA-693 S35000 - Detail

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Mechanical properties of grade SA-693 S35000 SA-693

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
253 (≥) 992 (≥) 12 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade SA-693 S35000 SA-693

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
899 (≥) 676 (≥) 12 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
846 472 225