SA-693 S45500 Stainless Steels to SA-693

SA-693 S45500 - Specification & Application

  • SA-693 - Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of SA-693 S45500 grade: to SA-693

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Mn - 0.50
Si - 0.50
P - 0.04
S - 0.03
Cr 11.00 12.50
Ni 7.50 9.50
Mo - 0.50

SA-693 S45500 - Detail

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Mechanical properties of grade SA-693 S45500 SA-693

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
954 (≥) 665 (≥) 14 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade SA-693 S45500 SA-693

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
329 (≥) 128 (≥) 11 13 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
316 587 296

Equivalent Products

We can customize the production of SA-693 S45500 grade, contact us for the best solution.