STS631 Stainless Steels to D 3534 (2002)

STS631 - Specification & Application

  • D 3534 (2002) - Cold rolled stainless steel strip for springs
  • D 3698 (2008) - Cold rolled stainless steel plates, sheets and strip
  • D 3705 (2008) - Hot rolled stainless steel plates, sheets and strip
  • D 3706 (2008) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of STS631 grade: to D 3534 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Ni 6.50 7.75
Mo - -
N - -
Al 0.75 1.50

STS631 - Detail

Stainless steel bars

Mechanical properties of grade STS631 D 3534 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
354 (≥) 427 (≥) 44 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade STS631 D 3534 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
253 (≥) 229 (≥) 43 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
287 786 671

Equivalent Products

We can customize the production of STS631 grade, contact us for the best solution.
sales@specificsteel.com