SUS309STP Special Alloy

Chemical composition%of the ladle analysis of gradeSUS309STP

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)
Max 0.08Max 1.00Max 2.00Max 0.04Max 0.032.00-24.0012.00-15.00
SUS309STP

Mechanical properties of gradeSUS309STP

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
228(≥) 635(≥) 14 31 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 133

Physical properties of grade SUS309STP

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
743(≥) 673(≥) 13 44 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
855 354 487

SUS309STP Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

SUS309STP Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
Incoloy800 round bar Φ115*1400 Round Bar Kgs 169 Hot-Rolled+Annealed+black Enquiry
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry
15-5PH Forgrd Flat Bar Select 0 Select Enquiry