DIN 17224 (1982) Stainless steel wire and strip for springs; technical delivery conditions; Replaced by DIN EN 10151:2003; DIN EN 10270-3:2001
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.07 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.015 | ||
Cr | 16.5 | 18.5 | ||
Mo | 2.00 | 2.50 | ||
Ni | 10.0 | 13.0 |
DIN 17224 (1982) Stainless steel wire and strip for springs; technical delivery conditions; Replaced by DIN EN 10151:2003; DIN EN 10270-3:2001
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
682 (≥) | 643 (≥) | 32 | 23 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
679 (≥) | 657 (≥) | 14 | 43 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
194 | 747 | 497 |
We can customize the production of X5CrNiMo-18-10 grade, contact us for the best solution.