Steels of blade for steam turbine
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.1500 | 0.2000 | ||
Mn | 0.5000 | 0.8000 | ||
P | - | 0.0200 | ||
S | - | 0.0150 | ||
Si | - | 0.5000 | ||
Ni | 0.3000 | 0.6000 | ||
Cr | 10.0000 | 12.0000 | ||
Mo | 0.6000 | 0.9000 | ||
Cu | - | 0.1000 | ||
V | 0.2000 | 0.3000 | ||
Al | - | 0.0300 | ||
N | 0.0400 | 0.0900 | ||
Nb | 0.2000 | 0.6000 |
S47670
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
259 (≥) | 377 (≥) | 12 | 42 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
265 (≥) | 228 (≥) | 33 | 13 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
933 | 567 | 932 |
We can customize the production of S47670 grade, contact us for the best solution.