A 249 S31040 Stainless Steels to A 249/A 249M (2010)

A 249 S31040 - Specification & Application

  • A 249/A 249M (2010) - Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of A 249 S31040 grade: to A 249/A 249M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.50
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - -
Nb+Ta 10×C% 1.10

A 249 S31040 - Detail

Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade A 249 S31040 A 249/A 249M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
356 (≥) 823 (≥) 13 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade A 249 S31040 A 249/A 249M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
995 (≥) 485 (≥) 44 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
832 873 978