B 691 N08366 Stainless Steels to B 691 (2002)

B 691 N08366 - Specification & Application

  • B 691 (2002) - Iron-Nickel-Chromium-Molybdenum Alloys (UNS N08366 and UNS N08367) Rod, Bar, and Wire

Iron-Nickel-Chromium-Molybdenum Alloys (UNS N08366 and UNS N08367) Rod, Bar, and Wire

Chemical composition(wt.%) of B 691 N08366 grade: to B 691 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.035
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.03
Cr 20.00 22.00
Ni 23.50 25.50
Mo 6.00 7.00

B 691 N08366 - Detail

Iron-Nickel-Chromium-Molybdenum Alloys (UNS N08366 and UNS N08367) Rod, Bar, and Wire

Mechanical properties of grade B 691 N08366 B 691 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
765 (≥) 352 (≥) 21 11 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade B 691 N08366 B 691 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
919 (≥) 796 (≥) 32 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
957 938 935

Equivalent Products

We can customize the production of B 691 N08366 grade, contact us for the best solution.