HR5 Stainless Steels to BS 2HR 5 (2010)

HR5 - Specification & Application

  • BS 2HR 5 (2010) - Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)
  • BS HR 5 - Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)

Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)

Chemical composition(wt.%) of HR5 grade: to BS 2HR 5 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 1.00
Mn - 1.00
P - -
S - 0.020
Cr 18.00 21.00
Ni - remaining
Mo - -
Co - 5.00
Ti 0.20 0.60
Fe - 5.00
Al - -
Cu - 0.50
B - -
Bi - -
Pb - 0.0050
Ag - -

HR5 - Detail

Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)

Mechanical properties of grade HR5 BS 2HR 5 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
312 (≥) 449 (≥) 31 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade HR5 BS 2HR 5 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
643 (≥) 689 (≥) 32 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
142 929 482

Equivalent Products

We can customize the production of HR5 grade, contact us for the best solution.