Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.005 | 0.02 | ||
Si | - | 0.75 | ||
Mn | - | 2.00 | ||
P | - | 0.04 | ||
S | - | 0.03 | ||
Ni | 9.00 | 13.00 | ||
Cr | 17.00 | 20.00 | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
N | 0.06 | 0.10 | ||
Mo | - | - | ||
V | - | - |
Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
311 (≥) | 847 (≥) | 14 | 11 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
791 (≥) | 353 (≥) | 32 | 31 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
536 | 572 | 328 |
We can customize the production of A 193 347LN Class 1 grade, contact us for the best solution.
–sales@specificsteel.com