  • A 213/A 213M (2011) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of A 213 TP310HCb grade: to A 213/A 213M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.030
Cr 24.00 26.00
Ni 19.00 22.00
Nb+Ta - 1.10
Cu - 0.75

A 213 TP310HCb - Detail

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade A 213 TP310HCb A 213/A 213M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
183 (≥) 564 (≥) 24 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade A 213 TP310HCb A 213/A 213M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
578 (≥) 615 (≥) 21 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
735 665 729