Chemical composition(wt.%) of SA-312 TP310HCb grade: to SA-312/SA-312M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.030
Cr 24.00 26.00
Ni 19.00 22.00
Nb+Ta - 1.10
Cu - 0.75

SA-312 TP310HCb - Detail

Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Mechanical properties of grade SA-312 TP310HCb SA-312/SA-312M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
844 (≥) 164 (≥) 32 21 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade SA-312 TP310HCb SA-312/SA-312M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
451 (≥) 374 (≥) 12 11 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
178 596 131