SA-312 S32654 Stainless Steels to SA-312/SA-312M

SA-312 S32654 - Specification & Application

  • SA-312/SA-312M - Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of SA-312 S32654 grade: to SA-312/SA-312M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn 2.00 4.00
Si - 0.50
P - 0.03
S - 0.005
Cr 24.00 25.00
Ni 7.00 8.00
Cu 0.30 0.60
N 0.45 0.55

SA-312 S32654 - Detail

Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Mechanical properties of grade SA-312 S32654 SA-312/SA-312M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
213 (≥) 827 (≥) 34 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade SA-312 S32654 SA-312/SA-312M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
714 (≥) 638 (≥) 41 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
616 657 683