Marage 250 Stainless Steels to SAE AMS 6512G (2012)

Marage 250 - Specification & Application

  • SAE AMS 6512G (2012) - Steel, Bars, Forgings, Tubing, and Rings 18Ni - 7.8Co - 4.9Mo - 0.40Ti - 0.10Al Consumable Electrode Vacuum Melted, Annealed

Steel, Bars, Forgings, Tubing, and Rings 18Ni - 7.8Co - 4.9Mo - 0.40Ti - 0.10Al Consumable Electrode Vacuum Melted, Annealed

Chemical composition(wt.%) of Marage 250 grade: to SAE AMS 6512G (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.10
Mn - 0.10
Ni - 18.00
Cr - -
Al - 0.10
Cu - -
Ti - 0.40
Fe - -
Mo - 5.00
Co - 8.00

Marage 250 - Detail

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Mechanical properties of grade Marage 250 SAE AMS 6512G (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
557 (≥) 548 (≥) 24 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Marage 250 SAE AMS 6512G (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
551 (≥) 788 (≥) 32 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
985 577 686