Wire, Steel Welding, 18.5Ni - 8.5Co - 5.2Mo - 0.72Ti - 0.10Al, (Marage 300), Vacuum Melted, Environment Controlled Packaging
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Si | - | 0.10 | ||
Mn | - | 0.10 | ||
Ni | - | 18.00 | ||
Cr | - | - | ||
Al | - | 0.10 | ||
Cu | - | - | ||
Ti | - | 0.40 | ||
Fe | - | - | ||
Mo | - | 5.00 | ||
Co | - | 8.00 |
Wire, Steel Welding, 18.5Ni - 8.5Co - 5.2Mo - 0.72Ti - 0.10Al, (Marage 300), Vacuum Melted, Environment Controlled Packaging
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
881 (≥) | 494 (≥) | 34 | 42 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
846 (≥) | 734 (≥) | 12 | 32 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
863 | 283 | 569 |
We can customize the production of Marage 300 grade, contact us for the best solution.
–sales@specificsteel.com