NA1 Stainless Steels to BS 3071

NA1 - Specification & Application

  • BS 3071 - Specification for nickel-copper alloy castings

Specification for nickel-copper alloy castings

Chemical composition(wt.%) of NA1 grade: to BS 3071

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.50
Mn - 1.50
P - 0.030
S - 0.030
Cr - -
Mo - -
Ni - remaining
Cu 28.00 34.00

NA1 - Detail

Specification for nickel-copper alloy castings

Mechanical properties of grade NA1 BS 3071

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
491 (≥) 214 (≥) 11 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade NA1 BS 3071

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
181 (≥) 679 (≥) 34 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
566 628 645