S.126 Stainless Steels to BS S 126

S.126 - Specification & Application

  • BS S 126 - Specification for aircraft material. 23/14 chromium-nickel heat-resisting steel (niobium stabilized) (35 tonf/sq in: limiting ruling section 6 in)

Specification for aircraft material. 23/14 chromium-nickel heat-resisting steel (niobium stabilized) (35 tonf/sq in: limiting ruling section 6 in)

Chemical composition(wt.%) of S.126 grade: to BS S 126

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 0.20 1.00
Mn 0.50 2.00
P - 0.035
S - 0.025
Cr 22.00 25.00
Ni 13.00 16.00
Mo - -
Nb - 8×C

S.126 - Detail

Specification for aircraft material. 23/14 chromium-nickel heat-resisting steel (niobium stabilized) (35 tonf/sq in: limiting ruling section 6 in)

Mechanical properties of grade S.126 BS S 126

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
115 (≥) 624 (≥) 24 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade S.126 BS S 126

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
244 (≥) 134 (≥) 24 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
111 298 293

Equivalent Grade

Equivalent Products

We can customize the production of S.126 grade, contact us for the best solution.