Specification for aircraft material. 23/14 chromium-nickel heat-resisting steel (niobium stabilized) (35 tonf/sq in: limiting ruling section 6 in)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | 0.20 | 1.00 | ||
Mn | 0.50 | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.025 | ||
Cr | 22.00 | 25.00 | ||
Ni | 13.00 | 16.00 | ||
Mo | - | - | ||
Nb | - | 8×C |
Specification for aircraft material. 23/14 chromium-nickel heat-resisting steel (niobium stabilized) (35 tonf/sq in: limiting ruling section 6 in)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
849 (≥) | 274 (≥) | 33 | 31 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
872 (≥) | 333 (≥) | 32 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
592 | 372 | 376 |
We can customize the production of S.126 grade, contact us for the best solution.