S.150 Stainless Steels to BS S 150

S.150 - Specification & Application

  • BS S 150 - Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)

Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)

Chemical composition(wt.%) of S.150 grade: to BS S 150

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.16
Si 0.15 0.60
Mn 0.30 1.20
P - 0.030
S - 0.025
Cr 9.80 11.20
Ni 0.60 1.20
Mo 0.40 0.80
Nb 0.15 0.45
V 0.10 0.25
N 0.030 0.075

S.150 - Detail

Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)

Mechanical properties of grade S.150 BS S 150

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
924 (≥) 298 (≥) 43 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade S.150 BS S 150

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
841 (≥) 999 (≥) 34 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
937 516 175

Equivalent Grade

Equivalent Products

We can customize the production of S.150 grade, contact us for the best solution.