Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.08 | 0.16 | ||
Si | 0.15 | 0.60 | ||
Mn | 0.30 | 1.20 | ||
P | - | 0.030 | ||
S | - | 0.025 | ||
Cr | 9.80 | 11.20 | ||
Ni | 0.60 | 1.20 | ||
Mo | 0.40 | 0.80 | ||
Nb | 0.15 | 0.45 | ||
V | 0.10 | 0.25 | ||
N | 0.030 | 0.075 |
Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
122 (≥) | 233 (≥) | 32 | 43 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
443 (≥) | 519 (≥) | 22 | 42 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
582 | 545 | 279 |
We can customize the production of S.150 grade, contact us for the best solution.