S31620 Stainless Steels

S31620 - Specification & Application

Austenitic Chromium Nickel Molybdenum Free-Machining Stainless Steel

Chemical composition(wt.%) of S31620 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.2
S 0.10 -
Cr 17.0 19.0
Ni 12.0 14.0
Mo 1.75 2.50

S31620 - Detail

Austenitic Chromium Nickel Molybdenum Free-Machining Stainless Steel

Mechanical properties of grade S31620

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
246 (≥) 824 (≥) 24 32 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade S31620

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
929 (≥) 256 (≥) 32 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
829 565 633