SUS316F Stainless Steels to SA/JIS G4303

SUS316F - Specification & Application

  • SA/JIS G4303 - Specification for stainless steel bars

Specification for stainless steel bars

Chemical composition(wt.%) of SUS316F grade: to SA/JIS G4303

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.2
S 0.10 -
Cr 17.0 19.0
Ni 12.0 14.0
Mo 1.75 2.50

SUS316F - Detail

Specification for stainless steel bars

Mechanical properties of grade SUS316F SA/JIS G4303

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
238 (≥) 781 (≥) 32 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade SUS316F SA/JIS G4303

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
828 (≥) 341 (≥) 24 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
424 741 994

Equivalent Products

We can customize the production of SUS316F grade, contact us for the best solution.
sales@specificsteel.com