E36-4 XES Aviation and Aero Steel to AIR 9160 C

E36-4 XES - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of E36-4 XES grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.55
Mn - 1.50
P - 0.040
S - 0.040
Al 0.02 -

E36-4 XES - Detail

E26-4 E 36-4 XES Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade E36-4 XES AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
618 (≥) 788 (≥) 34 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade E36-4 XES AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
413 (≥) 625 (≥) 43 41 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
144 154 396