wrought steels used in aeronautical constructions
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.20 | ||
Si | - | 0.55 | ||
Mn | - | 1.50 | ||
P | - | 0.040 | ||
S | - | 0.040 | ||
Al | 0.02 | - |
E26-4 E 36-4 XES Air 9160C wrought steels used in aeronautical constructions
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
891 (≥) | 795 (≥) | 22 | 21 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
424 (≥) | 494 (≥) | 43 | 33 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
432 | 625 | 584 |