2562 Stainless Steels to SS 142562

2562 - Specification & Application

  • SS 142562 - Stainless steel - SS steel 2562

Stainless steel - SS steel 2562

Chemical composition(wt.%) of 2562 grade: to SS 142562

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 19.00 21.00
Ni 24.00 26.00
Mo 4.00 5.00
Cu 1.20 2.00

2562 - Detail

Stainless steel - SS steel 2562

Mechanical properties of grade 2562 SS 142562

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
426 (≥) 393 (≥) 13 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade 2562 SS 142562

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
492 (≥) 854 (≥) 23 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
741 722 759

Equivalent Products

We can customize the production of 2562 grade, contact us for the best solution.
sales@specificsteel.com