EVl Stainless Steels

EVl - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EVl grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.45 -
Si 0.50 -
Mn 0.50 -
Cr 23.5 -
Ni 4.80 -
Mo 2.80 -

EVl - Detail

Steel for exhaust valves

Mechanical properties of grade EVl

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
431 (≥) 277 (≥) 22 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade EVl

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
276 (≥) 175 (≥) 12 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
559 349 192

Equivalent Products

We can customize the production of EVl grade, contact us for the best solution.