LWCF15 Stainless Steels to BS 6323-8

LWCF15 - Specification & Application

  • BS 6323-8 - Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Chemical composition(wt.%) of LWCF15 grade: to BS 6323-8

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si 0.20 1.00
Mn 0.50 2.00
P - 0.045
S - 0.030
Cr 17.50 19.00
Ni 8.00 11.00
Mo - -

LWCF15 - Detail

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Mechanical properties of grade LWCF15 BS 6323-8

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
177 (≥) 364 (≥) 41 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade LWCF15 BS 6323-8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
414 (≥) 976 (≥) 22 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
316 292 747

Equivalent Products

We can customize the production of LWCF15 grade, contact us for the best solution.