Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
S | - | 0.01 | ||
Si | - | 0.35 | ||
Cu | - | 0.25 | ||
Ni | 99 | - | ||
Fe | - | 0.4 |
Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C). Lower carbon content also reduces hardness, making Nickel 201 particularly suitable for cold-formed items.
STANDARD PRODUCT FORMS
Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3........................................................................0.321
g/cm3......................................................................... 8.89
Melting Range, °F ...................................................2615 – 2635
°C ...................................................1435 – 1446
Specific Heat, Btu/lb•°F ....................................................0.109
J/kg•°C........................................................... 456
Curie Temperature, °F ........................................................... 680
°C ........................................................... 360
Permeability ........................................................ Ferromagnetic
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........ 7.3
21 – 93°C, µm/m• °C............ 13.1
Thermal Conductivity, Btu • in/ft2•h•°F ........................... 550
W/m• °C.......................................... 79.3
Electrical Resistivity, ohm• circ mil/ft..................................51
µΩ•m..............................................0.085
TYPICAL MECHANICAL PROPERTIES
(Annealed)
Tensile Strength, ksi.............................................................. 58.5
MPa............................................................ 403
Yield Strength (0.2% Offset), ksi...........................................15
MPa..................................... 103
Elongation, % ..............................................................................50
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
252 (≥) | 558 (≥) | 22 | 24 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
312 (≥) | 265 (≥) | 42 | 33 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
978 | 153 | 689 |
We can customize the production of NICKEL 201 grade, contact us for the best solution.