NICKEL 201 Superalloys to UNS N02201

NICKEL 201 - Specification & Application

  • UNS N02201 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • ASME Code Case 2249 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • BS 3072 – 3074 (NA12) - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • ASTM B 160 – B 163, B 366,B 725, B 730, B 751,B 775, B 829 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • DIN 17740, 17750 – 17754 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • ASME SB-160 – SB-163,SB-366, SB-725, SB-730,SB-751, SB-775, SB-829 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
  • ISO 6207, 6208, 9723 – 9725 - Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.

Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.

Chemical composition(wt.%) of NICKEL 201 grade: to UNS N02201

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
S - 0.01
Si - 0.35
Cu - 0.25
Ni 99 -
Fe - 0.4

NICKEL 201 - Detail

Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C). Lower carbon content also reduces hardness, making Nickel 201 particularly suitable for cold-formed items.

STANDARD PRODUCT FORMS

Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.

PHYSICAL CONSTANTS AND THERMAL PROPERTIES

Density, Ib/in3........................................................................0.321
g/cm3......................................................................... 8.89
Melting Range, °F ...................................................2615 – 2635
°C ...................................................1435 – 1446
Specific Heat, Btu/lb•°F ....................................................0.109
J/kg•°C........................................................... 456
Curie Temperature, °F ........................................................... 680
°C ........................................................... 360
Permeability ........................................................ Ferromagnetic
Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........ 7.3
21 – 93°C, µm/m• °C............ 13.1
Thermal Conductivity, Btu • in/ft2•h•°F ........................... 550
W/m• °C.......................................... 79.3
Electrical Resistivity, ohm• circ mil/ft..................................51
µΩ•m..............................................0.085

TYPICAL MECHANICAL PROPERTIES
(Annealed)
Tensile Strength, ksi.............................................................. 58.5
MPa............................................................ 403
Yield Strength (0.2% Offset), ksi...........................................15
MPa..................................... 103
Elongation, % ..............................................................................50




Mechanical properties of grade NICKEL 201 UNS N02201

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
217 (≥) 749 (≥) 22 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade NICKEL 201 UNS N02201

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
639 (≥) 692 (≥) 11 44 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
329 484 273

Equivalent Grade

Equivalent Products

We can customize the production of NICKEL 201 grade, contact us for the best solution.