TUZ6CN18-09 Stainless Steels to NF A 49-117

TUZ6CN18-09 - Specification & Application

  • NF A 49-117 - Steel tubes. Seamless plain end tubes for pipes-lines and other uses. Ferritic and austenitic stainless steels. Dimensions. Technical delivery conditions
  • NF A 49-217 - Steel tubes. Seamless tubes for heat exchangers. Stainless ferritic, austenic or ferritoaustenitic steel grades. Dimensions. Technical delivery conditions
  • NF A 49-218 - Steel pipes. Seamless pipes for furnaces. Austenitic stainless steels. Dimensions (with normal or reduced tolerances). Technical delivery conditions

Steel pipes. Seamless pipes for furnaces. Austenitic stainless steels. Dimensions (with normal or reduced tolerances). Technical delivery conditions

Chemical composition(wt.%) of TUZ6CN18-09 grade: to NF A 49-117

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo - -
Ni 8.00 10.00

TUZ6CN18-09 - Detail

Steel pipes. Seamless pipes for furnaces. Austenitic stainless steels. Dimensions (with normal or reduced tolerances). Technical delivery conditions

Mechanical properties of grade TUZ6CN18-09 NF A 49-117

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
417 (≥) 692 (≥) 24 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade TUZ6CN18-09 NF A 49-117

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
361 (≥) 728 (≥) 32 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
195 796 862

Equivalent Products

We can customize the production of TUZ6CN18-09 grade, contact us for the best solution.
sales@specificsteel.com