Z6CN18-09 Stainless Steels to NF A 36-607

Z6CN18-09 - Specification & Application

  • NF A 36-607 - Austenitic stainless steel parts obtained by flat die forging or drop forging for boilers and pressure vessels. Grade and types
  • NF A 35-559 - Iron and steel. Heat treatable special steels and stainless steels for externally threaded fasteners for use at low temperatures
  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels
  • NF E 29-043 - Non alloy and alloy steel bolting for pressure equipement - Specifications
  • NF F 80-109 - Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Chemical composition(wt.%) of Z6CN18-09 grade: to NF A 36-607

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo - -
Ni 8.00 10.00

Z6CN18-09 - Detail

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Mechanical properties of grade Z6CN18-09 NF A 36-607

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
551 (≥) 572 (≥) 24 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Z6CN18-09 NF A 36-607

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
231 (≥) 216 (≥) 21 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
835 483 717

Equivalent Products

We can customize the production of Z6CN18-09 grade, contact us for the best solution.
sales@specificsteel.com