Rene 41 Stainless Steels to SAE AMS 5399D (2006)

Rene 41 - Specification & Application

  • SAE AMS 5399D (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution Heat Treated
  • SAE AMS 5545F (2010) - Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 54Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.5Al - 0.006B Vacuum Induction and Consumable Electrode Melted, Solution Heat Treatable Precipitation Heat Treated
  • SAE AMS 5712J (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable
  • SAE AMS 5713J (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated
  • SAE AMS 5800F (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 54Ni - 19Cr - 11Co - 10Mo - 3.2Ti - 1.5Al - 0.006B Vacuum Induction Melted
  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

These products have been used typically for parts requiring high strength up to 1600 °F (871 °C) and oxidation resistance up to 1800 °F (982 °C), but usage is not limited to such applications

Chemical composition(wt.%) of Rene 41 grade: to SAE AMS 5399D (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
Al 1.40 1.60
B 0.0030 0.0100
C - 0.12
Co 10.00 12.00
Cr 18.00 20.00
Cu - 0.50
Fe - 5.0
Mn - 0.10
Mo 9.0 10.50
Ni - Remainder
S - 0.0150
Si - 0.5000
Ti 3.0 3.3

Rene 41 - Detail

Rene 41

Mechanical properties of grade Rene 41 SAE AMS 5399D (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
234 (≥) 691 (≥) 12 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade Rene 41 SAE AMS 5399D (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
499 (≥) 159 (≥) 14 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
328 589 176

Equivalent Products