Rene 41 Stainless Steels to SAE AMS 5800F (2006)

Rene 41 - Specification & Application

  • SAE AMS 5800F (2006) - Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 54Ni - 19Cr - 11Co - 10Mo - 3.2Ti - 1.5Al - 0.006B

Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 54Ni - 19Cr - 11Co - 10Mo - 3.2Ti - 1.5Al - 0.006B

Chemical composition(wt.%) of Rene 41 grade: to SAE AMS 5800F (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 0.25
Mn - 0.25
Cr - 19.00
Ni - remaining
Mo - 10.00
Co - 11.00
W - -
Al - 1.50
Cu - -
Ti - 3.10
Fe - 1.80
B - 0.005

Rene 41 - Detail

Nickel Alloy, Corrosion and Heat-Resistant, Welding Wire 54Ni - 19Cr - 11Co - 10Mo - 3.2Ti - 1.5Al - 0.006B

Mechanical properties of grade Rene 41 SAE AMS 5800F (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
591 (≥) 184 (≥) 42 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade Rene 41 SAE AMS 5800F (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
631 (≥) 966 (≥) 14 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
483 416 487

Equivalent Products

We can customize the production of Rene 41 grade, contact us for the best solution.