Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 54Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.5Al - 0.006B Vacuum Induction and Consumable Electrode Melted, Solution Heat Treatable Precipitation Heat Treated
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.09 | ||
Si | - | 0.25 | ||
Mn | - | 0.25 | ||
Cr | - | 19.00 | ||
Ni | - | remaining | ||
Mo | - | 10.00 | ||
Co | - | 11.00 | ||
W | - | - | ||
Al | - | 1.50 | ||
Cu | - | - | ||
Ti | - | 3.10 | ||
Fe | - | 1.80 | ||
B | - | 0.005 |
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 54Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.5Al - 0.006B Vacuum Induction and Consumable Electrode Melted, Solution Heat Treatable Precipitation Heat Treated
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
128 (≥) | 754 (≥) | 44 | 14 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
133 (≥) | 886 (≥) | 44 | 41 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
521 | 438 | 175 |
We can customize the production of Rene 41 grade, contact us for the best solution.
–sales@specificsteel.com