A 167 S01815 Stainless Steels to A 167 (1999)

A 167 S01815 - Specification & Application

  • A 167 (1999) - Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of A 167 S01815 grade: to A 167 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.18
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Ni 14.00 15.50
Cr 17.00 18.50
Al - -
Cu - 0.50
Ti - -
Fe - -
V - -
Mo - -

A 167 S01815 - Detail

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Mechanical properties of grade A 167 S01815 A 167 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
618 (≥) 857 (≥) 33 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade A 167 S01815 A 167 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
696 (≥) 495 (≥) 13 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
167 242 711

Equivalent Products

We can customize the production of A 167 S01815 grade, contact us for the best solution.