A 269 S01815 Stainless Steels to A 269

A 269 S01815 - Specification & Application

  • A 269 - Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Chemical composition(wt.%) of A 269 S01815 grade: to A 269

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.18
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Ni 14.00 15.50
Cr 17.00 18.50
Al - -
Cu - 0.50
Ti - -
Fe - -
V - -
Mo - -

A 269 S01815 - Detail

Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Mechanical properties of grade A 269 S01815 A 269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
417 (≥) 235 (≥) 12 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade A 269 S01815 A 269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
162 (≥) 131 (≥) 12 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
816 375 265

Equivalent Products

We can customize the production of A 269 S01815 grade, contact us for the best solution.