X2CrNiMo18-15-4 Stainless Steels to SA/EN 10028-7

X2CrNiMo18-15-4 - Specification & Application

  • SA/EN 10028-7 - Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Chemical composition(wt.%) of X2CrNiMo18-15-4 grade: to SA/EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.18
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Ni 14.00 15.50
Cr 17.00 18.50
Al - -
Cu - 0.50
Ti - -
Fe - -
V - -
Mo - -

X2CrNiMo18-15-4 - Detail

Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Mechanical properties of grade X2CrNiMo18-15-4 SA/EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
297 (≥) 566 (≥) 31 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade X2CrNiMo18-15-4 SA/EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
539 (≥) 459 (≥) 12 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
881 458 995

Equivalent Products