A 646 Grade HP 9-4-20 Stainless Steels to A 646/A 646M (2011)

A 646 Grade HP 9-4-20 - Specification & Application

  • A 646/A 646M (2011) - Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Chemical composition(wt.%) of A 646 Grade HP 9-4-20 grade: to A 646/A 646M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.23
Si - 0.10
Mn - 0.20
Ni - 0.65
Cr - 0.40
Al 4.25 4.75
Cu - -
Ti - -
Fe - -
Mo - 0.85
Co 8.50 9.50
V 0.06 0.12
P - 0.01
S - 0.01
W 0.90 1.10

A 646 Grade HP 9-4-20 - Detail

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Mechanical properties of grade A 646 Grade HP 9-4-20 A 646/A 646M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
946 (≥) 463 (≥) 32 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade A 646 Grade HP 9-4-20 A 646/A 646M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
161 (≥) 811 (≥) 41 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
443 457 267

Equivalent Products

We can customize the production of A 646 Grade HP 9-4-20 grade, contact us for the best solution.