Steel, Bars, Forgings, Tubing, and Rings 1.0Cr - 7.5Ni - 4.5Co - 1.0Mo - 0.09V (0.29 - 0.34C) Consumable Electrode Vacuum Remelted, Annealed
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.29 | 0.34 | ||
Si | - | 0.10 | ||
Mn | 0.10 | 0.35 | ||
Ni | 7.00 | 8.00 | ||
Cr | 0.90 | 1.10 | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
Mo | 0.90 | 1.10 | ||
Co | 4.25 | 4.75 | ||
V | 0.06 | 0.12 | ||
P | - | 0.01 | ||
S | - | 0.01 |
Steel, Bars, Forgings, Tubing, and Rings 1.0Cr - 7.5Ni - 4.5Co - 1.0Mo - 0.09V (0.29 - 0.34C) Consumable Electrode Vacuum Remelted, Annealed
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
173 (≥) | 719 (≥) | 23 | 24 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
137 (≥) | 962 (≥) | 31 | 44 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
461 | 214 | 644 |
We can customize the production of HP 9-4-30 grade, contact us for the best solution.
–sales@specificsteel.com