Steel, Sheet, Strip, and Plate 0.75Cr - 9.0Ni - 4.5Co - 1.0Mo - 0.09V (0.17 - 0.23C) Vacuum Consumable Electrode Melted, Annealed
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.17 | 0.23 | ||
Si | - | 0.10 | ||
Mn | - | 0.20 | ||
Ni | - | 0.65 | ||
Cr | - | 0.40 | ||
Al | 4.25 | 4.75 | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
Mo | - | 0.85 | ||
Co | 8.50 | 9.50 | ||
V | 0.06 | 0.12 | ||
P | - | 0.01 | ||
S | - | 0.01 | ||
W | 0.90 | 1.10 |
Steel, Sheet, Strip, and Plate 0.75Cr - 9.0Ni - 4.5Co - 1.0Mo - 0.09V (0.17 - 0.23C) Vacuum Consumable Electrode Melted, Annealed
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
944 (≥) | 179 (≥) | 22 | 22 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
446 (≥) | 175 (≥) | 43 | 23 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
213 | 842 | 668 |
We can customize the production of HP 9-4-20 grade, contact us for the best solution.