Z6CN18-09F Stainless Steels to NF A 36-613

Z6CN18-09F - Specification & Application

  • NF A 36-613 - General purpose forgings. Stainless steels

General purpose forgings. Stainless steels

Chemical composition(wt.%) of Z6CN18-09F grade: to NF A 36-613

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 17.00 19.00
Mo - -
Ni 8.00 10.00

Z6CN18-09F - Detail

General purpose forgings. Stainless steels

Mechanical properties of grade Z6CN18-09F NF A 36-613

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
735 (≥) 219 (≥) 12 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade Z6CN18-09F NF A 36-613

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
273 (≥) 179 (≥) 33 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
153 493 584

Equivalent Products

We can customize the production of Z6CN18-09F grade, contact us for the best solution.