Rene 41 Stainless Steels to SAE AMS 5713J (2007)

Rene 41 - Specification & Application

  • SAE AMS 5713J (2007) - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated

Chemical composition(wt.%) of Rene 41 grade: to SAE AMS 5713J (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 0.25
Mn - 0.25
Cr - 19.00
Ni - remaining
Mo - 10.00
Co - 11.00
W - -
Al - 1.50
Cu - -
Ti - 3.10
Fe - 1.80
B - 0.005

Rene 41 - Detail

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution and Precipitation Heat Treated

Mechanical properties of grade Rene 41 SAE AMS 5713J (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
236 (≥) 245 (≥) 44 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade Rene 41 SAE AMS 5713J (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
397 (≥) 841 (≥) 34 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
691 225 979

Equivalent Products

We can customize the production of Rene 41 grade, contact us for the best solution.